Welcome to Shiv Ferro Cast

Cast Iron

Cast Iron Manufacturing Flow Chart

01

Raw Material

(Pig Iron + Steel Scrap + Ferroalloys + Recarburizer)

02

Melting Furnace-

(Induction Furnace melting at high temperature (~1350–1450°C))

03

Composition Control

(Carbon (C), Silicon (Si), Manganese (Mn) adjustment Remove impurities (Sulphur, Phosphorus control))

04

Pouring into Mould

(Sand mould prepared green sand / resin sand Molten metal poured into mould)

05

Solidification

(Controlled cooling to Formation of cast iron shape)

06

Shakeout & Cleaning

(Casting removed from mould Shot blasting / grinding for cleaning)

07

Inspection

( Dimensional check , Defect detection)

08

Finished cast Iron Casting

(cast Iron Casting ready for machining or use)